A good PETG printing guide starts with this: PETG usually prints best a little hotter than PLA, with a warmer bed, a slower first layer, and less aggressive cooling. For many printers, a strong starting point is 220–250°C nozzle, 70–85°C bed, 15–25 mm/s first layer speed, and moderate cooling instead of blasting the fan. That […]